ASTM A182 F5

Spread the love

ASTM A182 – Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High Temperature Service

Grade: F5

Chemical Requirements   max,%

Elements F5
Carbon 0.150
Manganese 0.30-0.60
Phosphorus 0.030
Sulfur 0.030
Silicon 0.50
Nickel 0.50
Chromium 4.0-6.0
Molybdenum 0.44-0.65

 

Tensile and Hardness Requirements

Grade F5
Tensile Strength,min, ksi [Mpa] 70[485]
Yield Strength, min,ksi [MPa] 40[275]
Elongation in 2 in.[50 mm] or 4D,min, % 20
Reduction of Area, min, % 35
Brinell HardnessNumber 143-217