ASTM A312 TP316
Chemical Requirements: Composition, %, max
| Grade | TP316(S31600) | 
| Carbon | 0.08 | 
| Manganese | 2.00 | 
| Phosphorus | 0.045 | 
| Sulfur | 0.030 | 
| Silicon | 1.00 | 
| Chromium | 16.0-18.0 | 
| Nickel | 11.0-14.0 a | 
| Molybdenum | 2.00-3.00 | 
a For welded TP316 pipe, the nickel range shall be 10.0–14.0 %.
Heat Treating Temperature: 1900 °F [1040 °C]
Tensile Requirements:
| Tensile Strength, min ksi [MPa] | 75 [515] | 
| Yield Strength, min ksi [MPa] | 30 [205] | 
Elongation in 2 in. or 50 mm (or 4D), min, %:
| Longitudinal | 35 | 
| Transverse | 25 |